Alloying niobium with 1% zirconium increases the strength of niobium, and decreases slightly its elongation. The increased strength is very advantageous especially at temperatures above 600 °C
Cold rolled, Annealed
Thickness: 0.5 mm to 50 mm
Width and length: 1000 x 2000 mm or cut to size
ASTM B393, ASTM B395